It enhances the bonding effect between the composite cement and the ceramic bonding surface.
Ips ceramic etching gel instructions for use.
Of page 1 49 0 p310 immediately call a poison center doctor.
Ips ceramic etching gel conditioning 60 sec with.
The ips ceramic etching gel is used for the creation of retentive bonding surfaces for the composite cementation technique.
The etch pattern results in enhanced bonding strength between the cementation material and the glass ceramic.
Hydrofluoric acid is highly toxic.
Ivoclar recommends preparing the glass with ips ceramic etching gel a 5 hydrofluoric acid for a maximum of 20 seconds.
Do not rely on the appearance of the internal surface as an indicator of adequate etching as a frosty appearance actually indicates over etching.
To osha hcs printing date 04 26 2017 reviewed on 04 26 2017version number 15 43 0 9 1 identification product identifier trade name.
It enhances the bonding effect between the luting composite and the ceramic bonding surface.
Ips ceramic etching gel application of the substance the mixtureetching gel for dental ceramic details of the supplier of the safety data sheet manufacturer supplier.
P321 specific treatment see on this label.
Ips ceramic etching gel contd.
Ips ceramic etching gel 20 s is used to generate retentive bonding surfaces on all ceramic restorations in preparation for incorporation.
Ips ceramic etching gel 5ml 30g.
Please read the corresponding instructions for use.
Page 1 10 safety data sheet acc.
Ivoclar vivadent all ceramics preparing for cementation zirconium oxide supported ceramics.
Ceramic instructions for use description the use of ips ceramic etching gel generates retentive bonding surfaces on glass ceramic restorations as a preparation for cementation.
Generally glass ceramics are etched using ips速 ceramic etching gel.
The ips ceramic etching gel is used for the creation of retentive bonding surfaces for the composite cementation technique.
2 3 other hazards special safety notes for the use of ips ceramic etching gel.
Etching produces retentive bonding surfaces which increases the bond between the luting composite and the all ceramic.
Euh071 corrosive to the respiratory tract.